Rust on these original swing outs is generally the rule rather than the exception. So, how do you deal with the lower inside edge of the little channel that seats the glass when it is seriously corroded away. There's very little solid to weld even though the outer frame is surface only rust including the channel that the outside rubber flap fits in.
Is there any type of little channel for the two straight areas that can be spliced in with epoxy, tig or whatever?