Posted by Marty on Sunday, April 19, 2009 at 13:12:02 :
In Reply to: cadium spray paint posted by dave on Sunday, April 19, 2009 at 12:14:48 :
Several paint companies sell "Dull Aluminum"...that's as close as you'll get.
You can Cad plate split rings but you have to be sure they put them in their oven after they come out of the tank or they'll be brittle.